This test shall evaluate the safety performance of a battery in overcharge situations. The main safety risks during overcharge are the decomposition of the electrolyte, cathode and anode breakdown, exothermic decomposition of the solid electrolyte interphase (SEI) layer, separator degradation, and lithium plating, which can lead to self-heating of the battery and thermal runaway. The factors affecting the outcome of the test shall, as a minimum, include, the charging rate and the finally reached state of charge. The protection can be ensured either by voltage control (interruption after reaching the limit charging voltage) or current control (interruption after exceeding maximum charging current).